The Problem - Random Cracking in Concrete
Of the problems facing concrete contractors, random cracking is among the most costly and aggravating. Random cracking is particularly troubling because it immediately casts doubt on concrete quality, leading to owner dissatisfaction, callbacks and disputes.
The Solution - The Soff-Cut Ultra Early EntryT System
SOFF-CUT has the only Ultra Early EntryT dry-cutting system which controls random cracking through the early timing of the cut. With the SOFF-CUT Ultra Early EntryT method, control joints are cut within one to two hours after the finishing process, and before final set. The control joints are not as deep as the traditional method - as little as 25mm -and the chance of random cracks occurring is minimized.
How the System Works
As concrete hydrates and begins to set, it develops internal stresses. The objective in controlling random cracking is to relieve these stresses before they seek their own relief in the form of a random crack. The up-cutting rotation of the blade combines with the patented skid plate by applying pressure to the surface to prevent chipping or spalling.
With the SOFF-CUT system, sawing of control joints occurs in the Green ZoneT - within the first hour or two after finishing, as opposed to conventional sawing after final set. Only one system, SOFF-CUT, allows you to cut in the Green Zone as part of the finishing process in order to more effectively control random cracking.
|